MS 133: PART H8:2008
PAINTS AND VARNISHES - EVALUATION OF DEGRADATION OF COATINGS - DESIGNATION OF QUANTITY AND SIZE OF DEFECTS, AND OF INTENSITY OF UNIFORM CHANGES IN APPEARANCE - PART H8: ASSESSMENT OF DEGREE OF DELAMINATION AND CORROSION AROUND A SCRIBE (ISO 4628-8:2005, MOD)

This part of ISO 4628 specifies a method for assessing delamination and corrosion, caused by a corrosive
environment, around a scribe in a coating on a test panel or other test specimen.
NOTE An example of a corrosive environment is salt spray (fog) as used in the method of exposure described in
ISO 7253 or ISO 9227 (see the Bibliography).